profile - Razi University
Faculty Member of Razi University
Razi University
Reza Bakhtiari
Associate Professor / Engineering / Materials Engineering and Metallurgy
Master Theses
-
بررسي تجربي و عددي ميزان تاثير آسيب فرو رفتگي در صلاحيت سرويس دهي لوله هاي انتقال گاز
Iraj Goorani 2025 -
Simulation of the resistance TLP joining process for thin sections
Zahra Fadaei 2025This research investigates the transient liquid phase bonding process assisted by electric current for joining thin sections. The simulation of this process was conducted using COMSOL software in two systems: copper-carbon steel-copper and copper-tin-copper, with varying layer thicknesses. The primary objective was to analyze temperature distribution and atomic diffusion during the bonding process. The results showed that in the copper-carbon steel-copper system, the temperature at the center of the piece reached approximately 1590°C, sufficient to melt the interlayer. It was also observed that increasing the base layer thickness from 1 mm to 5 mm resulted in a higher final bonding temperature. Atomic diffusion analysis revealed that the maximum diffusion depth occurred with a base layer thickness of 1 mm and an interlayer thickness of 0.02 mm, reaching a depth of 0.252 mm. In the copper-tin-copper system, the center temperature of the sample reached approximately 766°C, adequate for melting the tin layer. Modeling indicated that in both systems, the sample remained at the final bonding temperature for over 95% of the bonding time, highlighting a unique advantage of this method. The results were validated by comparing them with experimental data available in the literature, showing good agreement. This research's findings can contribute to the optimal design of transient liquid phase resistance bonding processes for industrial applications, particularly in microelectronics.
-
Transient liquid phase (TLP) bonding to repair compressor blades of Ilam Gas Refinery
Arian Piri 2023 -
The effect of nanoparticles-containing interlayer on the mechanical properties of TLP joints for Al5083 alloy
Fatemeh Oustoar 2022Aluminum 3819 due to its good corrosion resistance and high strength-to-weight ratio in marine, military, pipe- It is widely used in pressure vessels, shipbuilding, refrigeration industries, oil rigs and gas transmission lines. among All aluminum alloys, alloy 3819 for all welded assemblies, tanks with the highest welding efficiency and maximum strength, connection of marine equipment, bridges, cargo ships, heavy ships and marine organizations, TV masts, grinding equipment, recycling machine body transfer equipment and wherever needed Corrosion resistance equipment is widely used. A Ag/Sn/Ag system to Shar et al connected with ultrasonic assistance and concluded that the acceleration of Ag atomic penetration with ultrasonic assistance is 6 3 times faster - - than the traditional TLP connection. Gio et al. fine-grained 4897 aluminum alloys with zinc interlayer TLP method with the help of ultrasonic bonding and reported that long ultrasonic time increases Zinc penetrates into aluminum. Li et al. for bonding Ag/Mg using ultrasonic assisted TLP method used and obtained the optimum shear strength of 68 MPa in a short period of 7 seconds. At This research has examined the TLP connection with the help of ultrasonics. This type of connection can not only connect with It provides high mechanical properties but also acts as a low temperature joining method. TLP with help Ultrasonic does not need shielding gas and can accommodate complex structures. Until today TLP It is used to connect different materials with the help of ultrasonic.
-
Investigation of corrosion resistance of stellite 6 alloy fabricated by laser metal deposition (LMD)
Mohammad Amiri 2022 -
Investigating the effect of seal wall thickness on seepage and rising forces Case study of tower dam
Malihe Hatami zargaran 2022 -
Investigation Of Biocompatibility Of TLP Joints In Co-Cr-Mo/Ti-6Al-4V System
Sadegh Tamassoki 2021Abstract: Ti-6Al-4V alloy with good tribological properties, low elastic modulus, high strength to weight ratio and Co-Cr-Mo alloy with excellent corrosion and abrasion resistance are used as metal biomaterials in artificial joints. In this study, the biocompatibility of the bimetallic system of Co-Cr-Mo and Ti-6Al-4V alloys, which are connected to each other through the transient liquid phase (TLP) process was evaluated. In this study, samples without coating and with hydroxyapatite coating were evaluated. The Phase composition, coating microstructure, corrosion resistance, metal ion release rate and cytotoxicity of samples were examined by using X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM), Polarization, Inductively Coupled Plasma (ICP) and MTT tests. The results showed the presence of uniform and nanometer coating on the coated samples. Examination of corrosion resistance in SBF solution and blood serum showed that CT1 sample without coating had optimal resistance (icorr = 1.01 ?Acm?2 in serum solution and icorr = 1.25 ?Acm?2 in body simulation solution) and also the resistance of coated samples It is much more desirable than uncoated samples and the best result was related to HAp-CT1 sample (icorr = 0.1 ?Acm?2 in serum solution and icorr = 0.08 ?Acm?2 in body simulation solution). The results of ICP test showed that the release rate of ions in 7, 14, 28 days was less than the allowable limit. By performing cytotoxicity test, it was observed that the death rate of cultured cells on the samples within 3 days was a desirable value and close to the control sample and had a significant difference of p <0.05. In addition, cell growth on CT1 sample increased during 3 days, which indicates the optimal biocompatibility of CT1 sample compared to other samples. The results of tests performed in this study showed that the samples have good biocompatibility and the best result is related to CT1 sample. It was also observed that the hydroxyapatite coating applied on the samples significantly increased the biocompatibility rate. Key Words: TLP bonding, Biocompatibility, Corrosion Resistance, Metal Ion Release, Cytotoxicity.
-
Improvement of Feature Extraction Unit in Speaker Recognition Systems
Sabiyye Azadbakht 2021 -
آبزدايي اتانول با استفاده از غشا ماتريس آميخته كيتوسان-نقاط كوانتوم اكسيد گرافن به وسيله تراوش تبخيري
Danial Chaghamirza 2021gt; In this study, pure chitosan membranes and its matrix mixed with nanoparticles of graphene oxide quantum dots (fabricated in this study) crosslinked with glutaraldehyde were used to dehydrate ethanol. High hydrophilicity of chitosan resulted in acceptable dehydration function of chitosan membrane in ethanol dehydration process. Also, due to the hydrophilic functional groups and good dispersion of graphene oxide quantum dots in the chitosan network, the mixed matrix membranes performed better dehydration than the chitosan membrane. Matrix membrane mixed in optimal loading of quantum dots graphene oxide (1.5 wt%) flux0.811 kg/m2h and separation factor of 801 for dehydration of water / ethanol mixture (90/10) at 40°C Showed that compared to chitosan membrane, the flux base increased by 84% and the separation coefficient increased 7.6 times
-
The effect of repair welding on microstructure changes and mechanical properties of ASTM A516 grade 70 steel
Yaser Rezaei 2021 -
Investigation of surface nano structuring of properties TLP joints
Lila Jamshidibakhtar 2020 -
Study the corrosion mechanisms on outlet piping of reactor V-401 in kermanshah oil refinery
Younes Mirzaei 2020 -
Investigating the effect of nanoparticles on strengthing the TLP joints for AZ31 alloy
Faeze Dehnavi 2019 -
Effect of nanoparticles parameters on wettability of the reservoir ston, under different temperatures and fluids
Milad Khosravi 2019 -
The effect of friction stir process on microstructure and mechanical propertiesof transeint liquid phase joints for304
HAMED NIKOOKAR 2019In this research, the AISI304 steel was bonded successfully with MBF-15 and MBF-80 interlayers by Transient Liquid Phase [1]method. Then friction stir process[2] was performed on the bond region and the effect of the process on microstructure and mechanical properties was investigated. The base metal and each of interlayers separately was assembled and the bonding operation was done in 11350c temperature for 20 min in a semi-vacuum environment furnace. Afterward Friction Stir process applied with using a designed tool made from tungsten carbide material. The process was accomplished with a milling machine. Rotating speed of tool was 600 Rpm/min and traverse speed was 10 mm/s. the process was applied at two side of the bond line. Processed and not processed samples were prepared and investigate with optical and scanning electron microscope. The microstructure of samples compared with each other. To analyze the composition and phase recognition energy dispersive spectrometry[3] and XRD was used. To evaluate the mechanical properties and the effect of FSP on it shear strength test and micro hardness performed. The microstructure evaluation showed that before FSP for each of interlayers, there were some eutectic phase in center of bond and residual phase in the diffusion zone of TLP. Before FSP, for MBF-15 interlayer, the central phase is Ni-Si, Fe-B, Ni-B and CrB4 in DAZ of TLP. The eutectic phases in the central zone of bond by MBF-80 interlayer are Fe-B-Ni-B and brittle Cr5B3 in DAZ. These eutectic and residual phases reduce the mechanical strength of the joint.FSP was applied as a technique to modify the distribution of alloying elements and intermetallic phases. Underneath of FSP route, 3 zones were formed: 1. Nugget zone that distribution of intermetallic is perfect. 2.Thermo Mechanically Affected Zone[4]. and. 3. Heat Affected Zone [5]that the quantity of intermetallic phases is reduced because of dissolution of eutectic and residual phase. The shear strength and hardness of the nugget zone after FSP will be better than before FSP for both interlayers. This improvement for joint with MBF-15 interlayer is better than MBF-80. And shear strength of joint with MBF-15 interlayer is close to base metal shear strength after the process.1-TLP2-FSP3-EDS
-
Corrosion resistance of TLP joints for IN738/IN738 and IN738/FSX414 system
Fateme Bolghadr 2018 -
Influence of repair welding on pitting and intergranular corrosion behavior of super duplex 2507 stainless steel in NaCl 3.5%
ELAHE Mansouri 2018 -
Modeling and simulation of gas permeation through mixed matrix membranes using Comsol
Mona Morovat 2018The natural gas contains many impurities, including water, carbon dioxide ( ), and so on. The presence of acid gases in natural gas will lead to a reduction in thermal value, which is why removing these gases from natural gas to a standard value will be important. Increasing permeability and selectivity are the most important goals of research in membrane field. One of the common ways to achieve these goals is to add inorganic particles to the polymeric matrix of membranes, which are called as mixed matrix membranes.In this work, we present simulation of the effective permeability of pure gas in mixed-matrix membranes (MMMs) by CFD. For this, we use the finite element method to simulate gas effective permeability based on constructing three-dimensional MMM models for solving Fick's diffusion equation to obtain the concentration profiles.Our simulation also indicate effects of various structural parameters, including the filler volume fraction, interface solubility ratio, and diffusivity ratio and filler size. And also result of simulation for effective permeability of MCM-41 fillers compared by effective medium theory (Maxwell model).Our approach shows improved predictions compared with the Maxwell model. Key words: Mixed Matrix Membrane, Gas separation, Simulation, Finite-element, Comsol
-
Design Of Ultra Wideband Low Noise Amplifier (LNA) With Current Reuse And Noise Cancelling Technique
Ali Hatami 2018Design Of Ultra Wideband Low Noise Amplifier (LNA) With Current Reuse And Noise Cancelling Technique
-
Transient liquid phase(TLP)bonding for dissimilar TI-6AL-4V/CO-CR-MO system
Asma Merati 2017The Ti-6Al-4V alloy with good tribiological characteristics, low elastic modulus, high strength to weight ratio and the Co-Cr-Mo with excellent resistance to corrosion and erosion, are practical as metal bio-materials in artificial joints. The Co-Cr-Mo alloy leads to reduced corrosion in the thigh joint and the Ti-6Al-4V alloy easily pairs up with surrounding bones and is therefore preferred for thigh stem. To build such a bimetal system, given the disparity of welding parameters, connection is a big hurdle. Different welding methods such as fusion welding, laser welding, hard and soft soldering, and penetration bonding for simillar and disimillar bonding of these alloys have been used. In this study, the transient liquid phase rocess has been used for the Ti-6Al-4V/Co-Cr-Mo dissimilar system in order to address the shortcomings of other welding methods and access mechanical properties comparable with base metal. In this method, samples were cut as cylinders with 8 mm in diameter and 5.7 mm in height and their surfaces were prepared for bonding. An copper interlayer was placed between the two surfaces as covering on cobalt sample, and a constant pressure of 1 MPa was applied to the samples using fixture. Next, the bonding set was exposed to heating in under-pressure stove with the different temperatures of 925, 950 and 975, considering the eutectic temperature of Ti-Cu (about 875 °C), for 5 to 120 minutes. On the connected samples, cross section cut was performed and the substructure was studied using optical microscope. Results suggested that as a result of the bonding, 3 zones of DAZ (diffusion-affected region), ASZ (athermally solidified zone), and ISZ (isothermally solidified zone) appear in the bonding point, with the length of these zones differing depending on conditions of performing the bonding, and as joint temperature and duration increases, the athermally solidified zone can be removed, thus leading to progressed isothermally solidification during the bonding. Cut test was used to investigate mechanical strength of the samples, with the maximum shear strength equal to 350 MPa, which is around 50% of the base metal, obtained for the bonding made at 950 °C and in duration of 2 hours. Also, the failure level of the samples was identified with the X-ray diffraction test and failure level combination was considered. Type of failure and elements present in different phases of sample cross-sections were investigated using scanning electron microscopy. Elements constituting present elements were identified via the EDS test, and element changes in the sample were obtained with linear analysis. Keywords: transient liquid phase (TLP), Ti-6Al-4V, Co-Cr-Mo, evaluation of microstructure, mechanical properties, copper interlayer
-
Microstructure-mechanical properties study of transient liquid phasa(TLP)bonding for CO-Cr-MO alloy
Zahra Jalilian 2017In this research, utilizing transient liquid phase (TLP) joining for bio as-cast Co-28Cr-6Mo alloy similar bonding was investigated. Due to the good abrasion resistance, high mechanical properties, adequate corrosion resistance, high biocompatibility, as well as lower prices than gold base alloys, these alloys are the most suitable for biomedical applications. To this end, the TLP connection was performed using a MBF-100 cobalt-based and MBM-60 nickel-based interfacial layer with a thickness of 25 microns under argon gas atmosphere conditions at 1175 ?C and 15 min, and 1160?C and 60 min, 1170?C and 30 minutes , 1170 ?C and 60 min, and 1170 ?C and 120 min. The MBF-60 nickel base MBF-60 interface was also subjected to ambient atmospheres and vacuum of torr at 950, 1000, 1050, 1100, 1170 and 1240 ?C.In order to test the mechanical properties of bonding, the bonded specimens were subjected to cutting tests. The results showed that the bond strength of MBF-100 interlayer at 1170 ° C and 2 h had the highest shear strength. The strength of sample bonding was reached 81% of base metal. Also, the effect of complete thermal solvent treatment at 1240 ° C and 4 h on shear bond strength was investigated. It was observed that at the same temperature and time, the complete solution sample had a higher strength than the bonding of as-cast samples in similar conditions. The highest bond strength was for MBF-60 at 1000 ° C and 2 h.Investigation of microstructural analysis of the bonding was done using optical microscope and scanning electron microscopy (SEM) and SEM-EDS analysis results. The results of the bonding samples of 1175?C and 15 min using MBF-100 interlayer indicated that the melting was done on the boundaries at a bonding. By increasing the bonding time to 2 h at 1170?C, the penetration rate expanded, resulting in uniformity of the bonding region compounds and reduction of the phases present in the bonding region, indicating the expansion of the isothermal solidification zone. Boride compounds were also found in this sample indicate their stability.In joining studies conducted with the MBF-60 interlayer, it was found that in the bonding sample at 1000 ° C and 2 h, according to the EDS analysis the compounds were isolated as Cr3P3, Crp, Cr12P7, and CoP, and the phases Spherical is also seen in the DAZ zone. At temperatures, 1170° C was also observed continuous eutectic compounds at the center of the joint. The standard homogenization carbides dissolution process was carried out at 1240 ° C for 4 h the temperature for 4 hours. According to the microstructure bonding, the undesired phases of the bonding zone were significantly reduced and the homogeneity was observed. At this temperature, the carbides were completely dissolved and the granularity formed in the bonding zone.
-
Production of nanocrystalline alloy by annealing of ((Fe40-Ni40)Si11,B7,Mo2) amorphous alloys.
Soudabeh Soury 2017 -
Failure analysis of API 5L X60 steel pipes and study the microstructure - brittle behavior relationship
Bakhtyar Zandi nawa 2017Abstract: The pipelines that are used in the petroleum industry tra ort gas and oil with content of sulfidric gas that intensifies the adsorption of hydrogen in the metallic surface provoking the absorption of hydrogen in the wall of the pipe, what can flow in a embrittlement processThe welding process and the manufacturing process can also facilitate entry of hydrogen into the steel.The work done by other researchers suggest several parameters in the hydrogen losses had an impact. For example, have shown that the microstructures ferritic microstructure of ferrite needle more resistant to damage by hydrogen. Also tempered martensite microstructure bainite structures to very fine particles, perlite and martensite shows better behavior. Impurities and inclusions as trapping hydrogen in steels resources to act. Manganese sulfide is known as a harmful impurities.In this project, API 5L X60 pipes used in oil refineries Ntg Bijar area Kermanshah related to oil and gas companies have been defeated West under analysis. It was found that impurities MnS significant role in the formation of cracks were HIC. So that all EDS analysis show the presence of these impurities left in the region. Studies also show that the microstructure of the steel microstructure ferrite - pearlite with a hardness of 210 Vickers is that in some parts of needle ferrite and ferrite Weidman Ashtatn was observed in some areas.
-
production and optimization of biopolymer using microoranism isolated from oil wastewater
Zeinab Samimi 2017 -
Deposition and evaluation of wear properties for nanoscale multilayer titanium.nitride basedcoatings
Omid Googoonani 2016 -
Microstructure and mechanical properties of transient liquid phase (TLP) joints for AL 5083 alloy using strengthening nanoparticles in interlayer
MEYSAM AZIZI 2016 -
The effect of homogenization process on the mechanical properties and microstructure of the TLP bonded FSX-414 / MBF80/IN738
Abbas Jahanbakhsh 2014